摘 要:沙棘浆加工中排放酚酸含量高的果渣,因其苦涩无法被饲料工业大量转化,利用其进行微晶纤维素制备是潜在可行的解决途径。试验以粗提沙棘渣纤维素为处理对象,使用商品型号S10041纤维素酶水解,选取液料比(m L∶g)、酶添加量(U/m L)、酶解时间(h)、酶解温度(℃)、缓冲液p H值、离心转速(r/min)、烘干温度(℃)以及纤维粉碎度(目)八个因素,通过单因素和Plackett-Burman因素筛选并经过最陡爬坡和Box-Behnken试验优化了酶解条件。随后对制得的微晶纤维进行结构分析。结果表明:在液料比为49∶1(m L∶g)、酶添加量68U/m L、酶解时间1.3h、离心转速3640r/min时制得的沙棘微晶纤维素聚合度为355±1.02,与棉微晶纤维素聚合度最为接近。方差分析表明四个选定因素对指标均产生独立影响,因素交互作用对指标影响不显著(P=0.10)。微观结构显示沙棘微晶纤维表面结构更疏松,红外图谱对比沙棘和棉花两种微晶纤维官能团结构相似。(https://www.daowen.com)

关键词:沙棘渣;微晶纤维素;纤维素酶;优化

Abstract:Residue with phenolic acid from seabuckthorn pulp processing were discharged and because of its bitterness and astringency,they can not be used by forage industry in large scale.Therefore,preparation of microcrystalline cellulose by seabuckthorn pulp seemed to be a potential and feasible solution.In this experiment,the crude seabuckthorn residue cellulose was treated by cellulase hydrolysis of commercial model S10041.Eight factors were selected,including liquid-material ratio(m L:g),enzyme addition(U/m L),hydrolysis time(h),hydrolysis temperature(℃),buffer p H value,centrifugal rotation speed(r/min),drying temperature(℃)and fiber crushing degree(item),and screened by single factor and lackett-Burman factor.The enzymatic hydrolysis conditions were optimized by the steepest climb and Box-Behnken test.Then the structure of the microcrystalline fibers was analyzed.The results showed that the degree of polymerization of Hippophae rhamnoides microcrystalline cellulose was 355+1.02 when the ratio of liquid to material was 49∶1(m L∶g),the amount of enzyme added was 68U/m L,the time of enzymatic hydrolysis was 1.3h,and the centrifugal speed was 3640r/min,which was the closest to that of cotton microcrystalline cellulose.The variance analysis showed that the four selected factors had independent effects on the indicators,but the interaction of factors had no significant effect on the indicators(P=0.10)。Microstructure showed that the surface structure of seabuckthorn microcrystalline fibers was looser,and the functional groups of seabuckthorn and cotton microcrystalline fibers were similar by infrared spectroscopy.

Keywords:seabuckthorn residue;microcrystalline cellulose;cellulase;optimization

短束状或粉末状并呈现多孔状。在中性和弱酸性条件下不溶解,也不溶于有机溶剂和油脂,在弱碱性条件下部分溶解、溶胀,易于羧甲基化、乙酰化、酯化。粉末状微晶纤维素可用作黏合剂,可作为医用外伤保护剂、药物缓释剂、汽车玻璃涂膜剂;颗粒状纤晶纤维素可作为香料油脂包埋剂,在果汁饮料生产中作为悬浮剂和稳定剂等。因沙棘果渣含有大量纤维素成分,试验拟利用其制备微晶纤维素,通过对酶解条件优化以及对制得的微晶纤维素进行结构分析,为沙棘果渣高效转化利用提供基础数据。